The melting temperature of plastics is an important physical property in any plastic fabrication process.
Whether you are injection molding, extruding or choosing plastic for any application, you must know its melting temperature.
In this article, we explore the melting temperature of these thermoplastic polymers in detail.
What is the Melting Point of Plastic

The melting temperatures of plastics range roughly from 100°C to over 300°C, depending on the specific polymer.
This variation is mainly attributed to the different molecular structures in each type of plastic material.
For example, some plastics soften gradually and melt because they are thermoplastics, making them easier to reshape. Others, which are thermosets, decompose instead of melting.
Why the Melting Point of Plastic Matters

· Preserves Material Properties
During melting, the plastic is exposed to thermal damage, oxidation, and mechanical damage. This damages the molecular structure.
When the molecular structure is damaged, you might end up with inconsistent quality on your material, higher scrap rates, and reputation damage. Preserving the material properties will help you maintain and preserve, the molecular weight, thermal stability, chemical resistance, clarity and mechanical strength of your plastic.
· Helps with Material Selection
The melting point of plastic will help you determine if the material selected can undergo certain processing procedures that require high temperatures. It defines whether the plastic can even survive your operating environment.
You will also be able to control the risks of thermal degradation. Remember, low-melting plastics are easier to recycle and reprocess as compared to high-melting plastics. This means that you can be able to choose well which material to recycle or reprocess.
Here are out new series of plastic recycling machines.
· Facilitates Proper Processing
It will help you identify the safe zone between the melting temperature and degradation temperature. If the window is wide, your processing will be stable, and if your window is narrow, your processing will be fragile. In this zone, the polymer flows properly, fills the mold or die, and does not chemically degrade.
Proper processing means melting just enough. Every degree above leads to oxidation or chain scission. Paying attention to the right melting point degrees will help you prevent thermal damage.
· Averts Material Degradation
Every thermoplastic has a softening temperature where it becomes processable and a degradation temperature where chemical breakdown starts. The safe processing zone is between these two.
Therefore, melting point defines the lower limit of safe processing, and degradation defines the upper limit. It lets you set maximum safe temperatures and helps you prevent cumulative damage in reprocessing.
· Enhances Production Efficiency
It sets the minimum energy input required, where you cannot melt below the melting point. It also controls your cycle time and affects process stability.
Plastic melting point matters in enhancing production efficiency because it directly controls energy use. Remember the lower the melting point, the cheaper, faster, and more stable your production becomes.
Plastic Thermal Transition Stages

Whether you are extruding plastic material, or using it for any other application, you must understand the various thermal transition stages. These key stages include:
1. Glassy
Here, polymer chains are essentially frozen in place. The molecular motion is extremely limited, and the material behaves like a rigid solid. In this state, plastics show high modulus, high strength, but low toughness and low impact resistance, among others.
2. Rubbery
This is the temperature where the polymer chains gain segmental mobility. Here, chains can move and uncoil locally as the material is no longer rigid and brittle. Your plastic becomes tough, flexible, and ductile. Rubber polymer segments rotate and slide, redistributing stress instead of storing it. This means rubber plastics are not likely to shatter; however, they can deform.
3. Viscous
This is the temperature region where polymer chains have enough mobility to slide past each other freely. Plastic in this state can flow under pressure, fuse into a continuous shape, and fill molds, dies, and cavities.
In this state, plastic becomes a non-Newtonian, viscoelastic fluid depending on temperature, pressure, shear rate, and time. At viscous temperatures, polymer chains have enough energy to disentangle and move, creating a controlled flow which enables processing and quality control.
4. Decomposition
During decomposition, polymer chains undergo scission, their chemical bonds are destroyed, and the material loses its designed properties permanently. It destroys the mechanical performance where tensile strength drops, impact resistance collapses, and creep increases. It destroys appearance and creates environmental risks.
Types of Plastics According to Their Thermal Behavior

Remember, even as you choose a plastic extruder, one of the key variables you must consider is the melting temperature.
Therefore, in this section, we will focus on the melting temperature of the most common engineering plastic materials:
Low-Temperature Plastics
· Low-Density Polythene
The melting point range of LDPE is 105°C to 115°C with practical processing temperatures of 160°C to 200°C. This is because you will need more thermal energy to reduce viscosity for the LDPE to flow well.
· High-Density Polythene
HDPE usually has very little chain branching but has high crystallinity and a higher density. Because of its high crystallinity nature, HDPE has a high melting point that ranges between 130°C to 137°C with a processing temperature range of 180°C to 230°C. this makes it tougher and hotter.
· Polystyrene
Polystyrene has no crystalline regions. Its transitions from solid to molten state mainly is via the glass transition temperature of around 100°C. Polystyrene chains are bulky and rigid because of the phenyl benzene side groups that increase stiffness and reduce mobility making it brittle. On its thermal behavior, it does not melt. It softens then flows.
Mid-Temperature Plastics
· Polyvinyl Chloride
PVC has a strong intermolecular force due to its polar C–Cl bonds. It softens gradually but decomposes very close to its softening range. This makes it thermally unstable compared to most plastics. Its melting point is through, a glass transition of around 80°C with a processing window of about 160–200°C.
· Polypropylene
Polypropylene is a semi-crystalline thermoplastic that has a sharp melting point of 160–170°C. it has a wide processing window and melts cleanly, hence doesn’t decompose near its melting point.
· Polyoxymethylene
This plastic has a high crystallinity of 75–85% with a strong intermolecular bond. POM is rubbery at room temperature and melts at 165–175°C. It degrades rapidly when overheated and releases formaldehyde gas.
High-Temperature Plastics
· Polycarbonate
PC is an amorphous thermoplastic that transitions through a glass transition into a soft, rubbery, and then viscous state. PC keeps its stiffness and shape at elevated temperatures at a very high glass transition around 145°C with a processing temperature range around 260–320°C, and thermal degradation above roughly 320°C.
· Nylon 6
It is a semi-crystalline thermoplastic with strong hydrogen bonding between chains. Its melting point is 215–225°C and a low glass transition temperature of 45–55°C. its rubbery region at room temperature, and a relatively high processing temperature around 230–270°C.
· Polyethylene Terephthalate
This is a semi-crystalline thermoplastic polyester that has strong intermolecular interactions and has a high sensitivity to moisture and thermal history. Its melting point range is 250–260°C.
High Temperature Performance Plastics
· PTFE
PTFE crystallizes at a melting point of ~327°C. It does not flow like molten plastic, does not become processable by melting and decomposes before it ever becomes a true liquid. It is processed by pressing, sintering below decomposition. This means PTFE’s strength is thermal and chemical stability, not processability.
· Polyimide
Polyimides have rigid aromatic backbones, strong intermolecular interactions, and often partially crosslinked structures. This makes them ultra- high temperature thermoplastics. It
· PEEK
Polyether Ether Ketone is a semi-crystalline, high-performance thermoplastic. It stays rigid until 143 °C, stays in rubber form then suddenly melts at 343 °C. at room temperature it remains solid, stable, with an excellent mechanical strength. It loses stiffness at the rubbery stage then transitions sharply to melting.
What Affects the Melting Point of Plastics

· Polymer Chain Length
It increases intermolecular contact points and reduces chain mobility, causing the use of a lot of energy to separate chains, slightly increasing melting point.
Chain affects impact resistance, mechanical strength and melt viscosity of the polymer.
· Polymer Branching
Branching reduces crystallization, creating defects in the crystal lattice, leading to less energy needed to melt, hence lower temperature.
Short chain branching strongly lowers meting point making polymer more flexible.
Long chain branching increases melt elasticity and viscosity causing less effect on melting.
· Additives
They disrupt crystal packing and dilute the polymer lattice causing lower melting temperatures.
For instance, some additives lower effective melting but increases flexibility.
In some circumstances, they do not change polymer crystal structure directly, but can slightly alter the apparent melting by acting as heat sinks and changing crystallization behavior.
· Moisture Content
They reduce intermolecular forces by inserting between chains, causing stiffness.
Usually, it lowers molecular weights, reducing mechanical properties.
· Environmental Exposure
Oxygen attacks polymer chains, lowering molecular weights and viscosity.
As a result, there is UV degradation, where bonds are broken, creating free radicals, leading to chain scission.
Again, chemical exposure to solvents, fuels and oils can cause Tg and apparent softening temperature drop. This will also lead to crystallinity changes.
· Manufacturing Technology
Processing may affect the orientation of chains, distribution of additives, degree of degradation, and crystallinity levels, which may either increase or reduce the melting temperatures.
Shear and flow during processing, where high shear aligns chains and promotes crystallization. This can slightly raise the melting peak and narrow the transition.
· Crystallinity
Crystallinity raises melting point by close chain packing, strong intermolecular forces, and regular geometry. This results to the need for more energy to disrupt them, raising the melting temperature and a sharper melting peak.
Comparing the Melting Points of Different Plastics

| Plastic Type | Melting Point |
| TPU | 160–220 degrees depending on soft or hard segment ratio |
| PE | 130–135 degrees |
| PVC | Tg ~80, decomposes ~200 |
| PS | Tg ~100 |
| PP | 160–165 degrees |
| PET | 250–255 degrees |
| PC | Tg ~147 |
| Nylon | 220–225 |
| PMMA | Tg ~105 |
| PTFE | 327 degrees |
| PI | >500 |
| PEEK | 343 degrees |
| POM | 175–180 degrees |
FAQs

Which plastic has the highest melting point?
PEEK has the highest melting point of 343 °C
What is the difference between plastic melting point and plastic heat deflection temperature?
Plastic melting point is the temperature at which plastic loses its ordered structure. They then transition from solid to molten form or viscous melt that can flow.
Heat Deflection Temperature is the temperature at which a plastic deforms or stops behaving as a rigid structural material under a load.
Which plastic has the lowest melting point?
Low-Density Polyethylene (LDPE) has the lowest melting point of 105–115 °C.
Which kind of plastic does not melt?
Plastics that are thermosetting do not melt but decompose.
Will 170 °C degrees melt plastic?
Yes. Depending on the type of plastic. 170 °C will melt some plastics, soften others, do nothing to some.
Which type of plastic cannot be re-melted?
Thermosetting plastics cannot be re-melted.
At what temperature will plastic crack?
Plastic will crack when the polymer becomes brittle or the applied stress exceeds its ability to deform.
Does cold temperature degrade plastic?
Cold temperatures do not degrade plastics but make them brittle, causing them to easily crack or fail.
How does the plastic melting point affect industrial processes?
Melting point does not affect industrial processes. It determines which machines you can use, how fast you can run, how much energy you burn and the possible defects.
How do you test plastic melting point?
You test the plastic melting point by differential scanning calorimetry which measures heat flow into the polymer as temperature increases.
Why Choose Wecoex Plastic Extruders

At Wecoex, we have specially engineered plastic extrusion machines designed to meet your unique production requirements. Whether you process requires conical twin screw extruder, parallel twin screw extruder, or co-extrusion machines, we optimize every machine to match your unique plastic processing needs.
Tell us more about your project needs and we will customize extruder machine for your plastic processing – talk to our engineers now.